Thermanit 625
Basic covered electrode
C Si Mn Cr Mo Ni Nb Fe
<0.04 <0.7 <1 21.5 9.5 Bal. 3.3 <2.0
Characteristics
and field of use
Materials
Typical analysis
in %
TüV certified parent metals
X10NiCrAlTi32-20 H, X10NiCrAlTi32-20 (1.4876),
NiCr22Mo9Nb (2.4856), X2NiCrMoCu (1.4539),
X2CrNiMoCuN VdTüV-WBL. 473;
Alloy 600, Alloy 625, Alloy 800, 9% Ni steels
Stainless; high resistance to corrosive environments. Resistant
to stress corrosion cracking. Resistant to scaling up to 1100 °C
(2012 °F). Temperature limit: 500 °C (932 °F) max. in
sulphureous atmospheres. High temperature resistant up to
1000 °C (1832 °F). Cold toughness at subzero temperatures
as low as –196 °C (–321 °F). For joining and surfacing work
with matching/similar corrosion resistant materials as well as on
matching and similar heat resistant, high temperature steels
and alloys. For joining and surfacing work with cryogenic
austenitic CrNi(N) steels/cast steel grades and on cryogenic
Ni steels suitable for quenching and tempering.