A32造船板一般强度船体结构钢力学性能与化学成份
钢材级别 |
屈服点不小于 |
抗拉强度 |
伸长率σ% 不小于 |
碳 C |
锰 |
硅 Si |
硫 S |
磷 P |
A |
235 |
400-520 |
22 |
≤0.21 |
≥2.5 |
≤0.5 |
≤0.035 |
≤0.035 |
B |
≤0.21 |
≥0.80 |
≤0.35 |
|||||
D |
≤0.21 |
≥0.60 |
≤0.35 |
|||||
E |
≤0.18 |
≥0.70 |
≤0.35 |
高强度船体结构钢力学性能与化学成份
钢材级别 |
屈服 不小于 |
抗拉强度 |
伸长率σ% 不小于 |
碳 C |
锰 |
硅 Si |
硫 S |
磷 P |
A32 |
315 |
440-570 |
22 |
≤0.18 |
≥0.9-1.60 |
≤0.50 |
≤0.035 |
≤0.035 |
D32 |
||||||||
E32 |
||||||||
F32 |
≤0.16 |
≤0.025 |
≤0.025 |
|||||
A36 |
355 |
490-630 |
21 |
≤0.18 |
≤0.035 |
≤0.035 |