NORYL PPO EXNL0140物性表
热塑性塑料,汽车电线绝缘nonhalogenated材料类C
TYPICAL PROPERTIES (1)
MECHANICAL 机械性能
Value Unit Standard
Tensile Stress, yld, Type I, 50 mm/min / 抗拉强度,屈服,类型I,50 mm/min
43
MPa
ASTM D 638
Tensile Stress, brk, Type I, 50 mm/min / 抗拉强度, 断裂, 类型I, 50 mm/min
41
MPa
ASTM D 638
Tensile Strain, yld, Type I, 50 mm/min / 拉伸伸长, 屈服, 类型I, 50 mm/min
9.7
%
ASTM D 638
Tensile Strain, brk, Type I, 50 mm/min / 拉伸伸长,断裂,类型I, 50 mm/min
62
%
ASTM D 638
Tensile Modulus, 50 mm/min / 拉伸模量,50 mm/min
1590
MPa
ASTM D 638
Flexural Stress, yld, 1.3 mm/min, 50 mm span / 挠曲强度, 屈服, 1.3 mm/min, 50 mm 跨距
54
MPa
ASTM D 790
Flexural Modulus, 1.3 mm/min, 50 mm span / 挠曲模量, 1.3 mm/min, 50 mm 跨距
1560
MPa
ASTM D 790
IMPACT
Value Unit Standard
Izod Impact, notched, 23°C / 悬臂梁缺口冲击强度23°C
328
J/m
ASTM D 256
THERMAL
Value Unit Standard
HDT, 1.82 MPa, 3.2mm, unannealed / 热变形温度,1.82 MPa, 3.2mm,未退火
90
°C
ASTM D 648
PHYSICAL
Value Unit Standard
Specific Gravity/比重
1.03
-
ASTM D 792
Melt Flow Rate / 熔流率, 280°C/5.0 kgf
13.8
g/10 min
ASTM D 1238
Source GMD, last updated:
Processing
Parameter
Wire Coating Extrusion
Value Unit
Drying Temperature / 干燥温度
40 - 80
°C
Drying Time / 干燥时间
0 - 6
hrs
Drying Time (Cumulative) / 干燥时间(累积的)
8
hrs
Maximum Moisture Content / 含湿量
0.05
%
Screw Speed / 螺杆速度
5 - 50
rpm
Feed Zone Temperature
20 - 50
°C
Middle Zone Temperatures
230 - 250
°C
Head Zone Temperature
270 - 280
°C
Neck Temperature
270 - 280
°C
Cross-head Temperature
270 - 280
°C
Die Temperature / 模具温度
270 - 280
°C
Melt Temperature / 熔体温度
270 - 285
°C
Conductor Pre-heat Temperature
20 - 100
°C
Screen Pack
mesh 200 - 80
-
Cooling Water Air Gap
100 - 1000
mm
Water Bath Temperature
15 - 30
°C
TYPICAL PROPERTIES (1)
MECHANICAL 机械性能
Value Unit Standard
Tensile Stress, yld, Type I, 50 mm/min / 抗拉强度,屈服,类型I,50 mm/min
43
MPa
ASTM D 638
Tensile Stress, brk, Type I, 50 mm/min / 抗拉强度, 断裂, 类型I, 50 mm/min
41
MPa
ASTM D 638
Tensile Strain, yld, Type I, 50 mm/min / 拉伸伸长, 屈服, 类型I, 50 mm/min
9.7
%
ASTM D 638
Tensile Strain, brk, Type I, 50 mm/min / 拉伸伸长,断裂,类型I, 50 mm/min
62
%
ASTM D 638
Tensile Modulus, 50 mm/min / 拉伸模量,50 mm/min
1590
MPa
ASTM D 638
Flexural Stress, yld, 1.3 mm/min, 50 mm span / 挠曲强度, 屈服, 1.3 mm/min, 50 mm 跨距
54
MPa
ASTM D 790
Flexural Modulus, 1.3 mm/min, 50 mm span / 挠曲模量, 1.3 mm/min, 50 mm 跨距
1560
MPa
ASTM D 790
IMPACT
Value Unit Standard
Izod Impact, notched, 23°C / 悬臂梁缺口冲击强度23°C
328
J/m
ASTM D 256
THERMAL
Value Unit Standard
HDT, 1.82 MPa, 3.2mm, unannealed / 热变形温度,1.82 MPa, 3.2mm,未退火
90
°C
ASTM D 648
PHYSICAL
Value Unit Standard
Specific Gravity/比重
1.03
-
ASTM D 792
Melt Flow Rate / 熔流率, 280°C/5.0 kgf
13.8
g/10 min
ASTM D 1238
Source GMD, last updated:
Processing
Parameter
Wire Coating Extrusion
Value Unit
Drying Temperature / 干燥温度
40 - 80
°C
Drying Time / 干燥时间
0 - 6
hrs
Drying Time (Cumulative) / 干燥时间(累积的)
8
hrs
Maximum Moisture Content / 含湿量
0.05
%
Screw Speed / 螺杆速度
5 - 50
rpm
Feed Zone Temperature
20 - 50
°C
Middle Zone Temperatures
230 - 250
°C
Head Zone Temperature
270 - 280
°C
Neck Temperature
270 - 280
°C
Cross-head Temperature
270 - 280
°C
Die Temperature / 模具温度
270 - 280
°C
Melt Temperature / 熔体温度
270 - 285
°C
Conductor Pre-heat Temperature
20 - 100
°C
Screen Pack
mesh 200 - 80
-
Cooling Water Air Gap
100 - 1000
mm
Water Bath Temperature
15 - 30
°C