Elgiloy非磁性合金

  • 发布时间:2020-09-03 10:32:07,加入时间:2017年08月22日(距今2810天)
  • 地址:中国»上海»松江:松卫北路678号
  • 公司:通项金属材料(上海)有限公司,用户等级:普通会员 已认证
  • 联系:高乐遥,手机:13816883178 电话:021-67860205 QQ:1031131415

Elgiloy®

UNS R30003

W.Nr 2.4711

Applications

Springs, seals, semiconductor components, orthodontics, medical devices, surgical implants, satellite communications equipment, and weapons systems.

Description

Elgiloy® is a non-magnetic Cobalt-Chromium-Nickel-Molybdenum alloy having a unique combination of very high strength while maintaining excellent formability, excellent corrosion resistance, and high fatigue strength. Additional strength increases of up to 25% can be achieved through aging cold reduced material. Elgiloy® is highly resistant to sulfide stress corrosion cracking, and as a result is the alloy of choice in the most demanding sour well environments. In seawater, Elgiloy® is virtually immune to crevice and stress corrosion and pitting even at the highest strength levels. Elgiloy® performs across a wide range of temperatures: from cryogenic up to 850°F (454°C).

Industries Supplied

Oil & Gas Extraction, Medical, Dental, Aerospace, Defense, Space Exploration and Watch making.

Nominal Composition

C: 0.15 max

Mn: 1.5 - 2.5

Si: 1.20 max

P: 0.015 max

S: 0.015 max

Cr: 19.0 - 21.0

Ni: 14.0 - 16.0

Co: 39.0 - 41.0

Mo: 6.0 - 8.0

Be: 0.10 max

Fe: Balance

Physical Properties

Density: 0.30 lb/in3, (8.30 g/cm3)

Modulus of Elasticity (E): 

At 70°F (20°C): 27.0 x 103 ksi (190 GPa)

Modulus of Rigidity (G): 

At 70°F (20°C): 11.0 x 103 ksi (76 GPa)

Coefficient of Expansion:

8.4 µin/in.-°F (70°F to 600°F)

15.2 µm/m-°C (20°C to 300°C)

Electrical Resistivity: 39.21 µΩ.in, (99.6 µΩ.cm)

Thermal Conductivity: 86.5 Btu-in/ft2hr-°F, (12.5 W/m-K)

Applicable Specifications

Strip and Foil: AMS 5876, ASTM F1058, NACE MR 0175 & MR 0103, ISO 5832-7

Typical Mechanical Properties – Spring Applications

Annealed

Heat Treatment: Per AMS 5876

Tensile Strength: 100 ksi min (690 MPa)

Suggested Operating Conditions: -300°F to 850°F (-184°C to 454°C)

Spring Temper

Heat Treatment: No Heat Treatment

Tensile Strength: Up to 310 ksi (2100 MPa)

Suggested Operating Condition­­s: -300°F to 850°F (-184°C to 454°C)

Spring Temper + Aged

Heat Treatment: After cold rolling. Age: Per AMS 5876, Nace MR 0175

Tensile Strength: Up to 380 ksi (2600 MPa)

Suggested Operating Conditions: -300°F to 850°F (-184°C to 454°C)

联系我时请说明来自志趣网,谢谢!

免责申明:志趣网所展示的信息由用户自行提供,其真实性、合法性、准确性由信息发布人负责。使用本网站的所有用户须接受并遵守法律法规。志趣网不提供任何保证,并不承担任何法律责任。 志趣网建议您交易小心谨慎。